Chemical Composition
0.5
%    
1.15
%    
95.1
%    (estimate)
0.75
%    
2.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1240 to 1760
MPa    
1280 to 2320
MPa    
9 to 14
% strain    
420 to 670
   
 
Other Information