Chemical Composition
0.3 to 0.5
%    
3 to 5
%    
73.3 to 79.7
%    (estimate)
17 to 19
%    
0.05 to 0.12
%    
1
%  (maximum)  
0.06
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 