Chemical Composition
0.3
%    
99.7
%    (estimate)
Cr, Ni, Mo
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
250 to 310
   
 
Other Information