Chemical Composition
0.35 to 0.42
%    
97.1 to 97.8
%    (estimate)
0.5 to 0.8
%    
0.007
%  (maximum)  
0.05
%  (maximum)  
0.05
%  (maximum)  
1.4 to 1.6
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 