Chemical Composition
3
%    
7.5
%    
89.5
%    (estimate)
Sn is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
100
   
 
Other Information
100 HB; Steel backed tin base babbitt. Used in refrigeration engineering and with high-alloyed lubricants. Corrosion resistant due to high tin content. SAE 12; DIN/ISO 4383.
GLYCO 38
 