Chemical Composition
0.08
%  (maximum)  
18.00 to 20.00
%    
2.00
%  (maximum)  
3.00 to 4.00
%    
11.00 to 15.00
%    
0.045
%  (maximum)  
0.030
%  (maximum)  
1.00
%  (maximum)  
 
Mechanical Properties
Other Information
Austenitic Cr-Ni-Mo Stainless Steel (317)
UNS S31700
UNS S31700
AISI 317 AMS AMS-QQ-S-763 ASME SA-240 (317); SA-249 (317); SA-312 (317); SA-403 (317); SA-409 (317) ASTM A1012 (TP317); A182 (F317); A213 (TP317); A240 (317); A249 (317); A269 (TP317); A276 (317); A312 (317); A314 (317); A403 (WP317); A409 (317); A473 (317); A478 (317); A479 (317); A511 (MT317); A554 (MT317); A580 (317); A632 (TP317); A813 (TP317); A814 (TP317); A943 (TP317); A988; F899 (317) SAE J405 (317)
Unified Numbering System (joint publication of ASTM and SAE)
 