Chemical Composition
0.08
%  (maximum)  
12 to 14
%    
83.2 to 88
%    (estimate)
1
%  (maximum)  
0.6
%  (maximum)  
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 