Chemical Composition
0.26 to 0.35
%    
12 to 14
%    
82.6 to 87.7
%    (estimate)
1
%  (maximum)  
1
%  (maximum)  
0.04
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 