Chemical Composition
0.03
%  (maximum)  
24 to 26
%    
41.2 to 50.7
%    (estimate)
5 to 7
%    
4 to 5
%    
0.3 to 0.6
%    
0.15
%  (maximum)  
16 to 19
%    
0.03
%  (maximum)  
0.015
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
420
MPa  (minimum)  
800 to 950
MPa    
35
% strain  (minimum)  
 
Other Information