Chemical Composition
3
%  (maximum)  
1 to 2.5
%    
0.5
%  (maximum)  
66.9 to 79
%    (estimate)
0.5 to 1.5
%    
18 to 22
%    
0.08
%  (maximum)  
0.5
%  (maximum)  
1.5 to 3
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
210
MPa    
370 to 440
MPa    
7
% strain    
140 to 200
   
 
Other Information