Chemical Composition
0.5 to 0.6
%    
1 to 1.2
%    
94 to 95.7
%    (estimate)
0.65 to 0.95
%    
0.45 to 0.55
%    
1.5 to 1.8
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
0.1 to 0.4
%    
0.07 to 0.12
%    
0.3
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
248
 (maximum)  
 