Chemical Composition
2.5
%  (maximum)  
1.5 to 4.5
%    
0.5
%  (maximum)  
62.5 to 75.5
%    (estimate)
0.5 to 1.5
%    
18 to 22
%    
0.5
%  (maximum)  
0.5
%  (maximum)  
4.5 to 5.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
190 to 280
MPa    
2
% strain    
140 to 250
   
 
Other Information