Chemical Composition
0.015 to 0.12
%    
0.13
%  (maximum)  
0.5 to 0.8
%    
0.2 to 0.5
%    
96.6 to 98.9
%    (estimate)
0.6
%  (maximum)  
0.01 to 0.06
%    
0.2 to 0.4
%    
0.04
%  (maximum)  
0.04
%  (maximum)  
0.15 to 0.5
%    
0.06
%  (maximum)  
0.02 to 0.1
%    
0.01 to 0.06
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
215
MPa    
360 to 490
MPa    
24 to 26
% strain    
 