Chemical Composition
0.03
%  (maximum)  
0.5 to 1.5
%    
23 to 26
%    
1
%  (maximum)  
55.2 to 69.4
%    (estimate)
2
%  (maximum)  
2 to 4
%    
0.08 to 0.25
%    
5 to 8
%    
0.04
%  (maximum)  
0.03
%  (maximum)  
2
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
450
MPa  (minimum)  
620
MPa  (minimum)  
20
% strain  (minimum)  
297
 (maximum)  
 
Other Information
Links



No warranty is given for the accuracy of these data