Chemical Composition
0.1 to 0.3
%    
0.08
%  (maximum)  
11.5 to 13.5
%    
0.3
%  (maximum)  
83.5 to 88.4
%    (estimate)
1
%  (maximum)  
0.3
%  (maximum)  
0.04
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
250
MPa  (minimum)  
440
MPa  (minimum)  
20
% strain  (minimum)  
187
 (maximum)  
88
 (maximum)  
 
Other Information