Chemical Composition
0.12
%  (maximum)  
17 to 19.5
%    
66.8 to 75
%    (estimate)
1.5
%  (maximum)  
8 to 10
%    
0.045
%  (maximum)  
0.03
%  (maximum)  
2
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
175
MPa    
440 to 640
MPa    
20
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data