Chemical Composition
0.05
%  (maximum)  
0.13 to 0.18
%    
11.5 to 13
%    
84.5 to 87.8
%    (estimate)
0.4 to 0.6
%    
0.2
%  (maximum)  
0.15 to 0.45
%    
0.5
%  (maximum)  
0.03
%  (maximum)  
0.03
%  (maximum)  
0.5
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
515
MPa  (minimum)  
795
MPa  (minimum)  
15
% strain  (minimum)  
277
 (maximum)  
 