Chemical Composition
0.02
%  (minimum)  
0.17
%  (maximum)  
97.1 to 100
%    (estimate)
2
%  (maximum)  
0.009
%  (maximum)  
0.04
%  (maximum)  
0.04
%  (maximum)  
0.6
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
185
MPa    
320 to 470
MPa    
21
% strain    
 
Other Information