Chemical Composition
0.15
%  (maximum)  
0.35
%  (maximum)  
0.5
%  (maximum)  
95.4 to 99.1
%    (estimate)
0.3 to 0.6
%    
0.44 to 0.65
%    
0.5
%  (maximum)  
0.04
%  (maximum)  
0.045
%  (maximum)  
0.15 to 1.65
%    
0.1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
4.28e6
lbf/ft^2  (minimum)  
8.67e6
lbf/ft^2  (minimum)  
22
% strain  (minimum)  
201
 (maximum)  
 
Other Information