Chemical Composition
0.04
%  (maximum)  
24.5 to 26.5
%    
2.75 to 3.25
%    
59.9 to 66.3
%    (estimate)
1
%  (maximum)  
1.75 to 2.25
%    
4.75 to 6
%    
0.04
%  (maximum)  
0.04
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
485
MPa  (minimum)  
690
MPa  (minimum)  
16
% strain  (minimum)  
 
Other Information