Chemical Composition
0.17 to 0.24
%    
0.4
%  (maximum)  
97.7 to 99.4
%    (estimate)
0.4 to 0.7
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.045
%  (maximum)  
0.045
%  (maximum)  
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
210
MPa  (minimum)  
410
MPa  (minimum)  
25
% strain  (minimum)  
 
Other Information