Chemical Composition
0.12 to 0.17
%    
0.8 to 1.1
%    
93.9 to 95.6
%    (estimate)
0.3 to 0.6
%    
0.2 to 0.3
%    
3 to 3.5
%    
0.035
%  (maximum)  
0.02 to 0.035
%    
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
790
MPa    
1150 to 1500
MPa    
8
% strain    
 
Other Information