Chemical Composition
0.13
%  (maximum)  
0.5 to 0.8
%    
0.2 to 0.5
%    
97 to 99
%    (estimate)
0.6
%  (maximum)  
0.2 to 0.4
%    
0.04
%  (maximum)  
0.04
%  (maximum)  
0.15 to 0.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
4.91e6
lbf/ft^2    
7.52e6 to 1.02e7
lbf/ft^2    
24 to 26
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data