Chemical Composition
0.17 to 0.23
%    
0.9 to 1.2
%    
97.2 to 98.3
%    (estimate)
0.6 to 0.9
%    
0.035
%  (maximum)  
0.02 to 0.035
%    
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
640
10^7 dyne/cm^2    
850 to 1200
10^7 dyne/cm^2    
10
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data