Chemical Composition
0.06 to 0.12
%    
0.3
%  (maximum)  
98.9 to 99.7
%    (estimate)
0.25 to 0.5
%    
0.045
%  (maximum)  
0.05
%  (maximum)  
0.05
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
343 to 490
MPa    
10
% strain  (minimum)  
 
Other Information
Links



No warranty is given for the accuracy of these data