Chemical Composition
0.52 to 0.6
%    
96.4 to 97.4
%    (estimate)
0.6 to 0.9
%    
0.04
%  (maximum)  
0.04
%  (maximum)  
1.5 to 2
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
285
 (maximum)  
 
Other Information
Links



No warranty is given for the accuracy of these data