Chemical Composition
0.13
%  (maximum)  
0.15
%  (maximum)  
0.2
%  (maximum)  
99.2 to 100
%    (estimate)
0.06
%  (maximum)  
0.005
%  (minimum)  
0.2
%  (maximum)  
0.06
%  (maximum)  
0.015
%  (maximum)  
0.005
%  (minimum)  
0.005
%  (minimum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
420 to 520
MPa    
520
MPa  (minimum)  
16
% strain  (minimum)  
 