Chemical Composition
0.34
%    
1.1
%    
97.3
%    (estimate)
0.75
%    
0.2
%    
0.03
%    
0.03
%    
0.25
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 