Chemical Composition
0.35 to 0.45
%    
97.4 to 98.3
%    (estimate)
1.3 to 1.7
%    
0.035
%  (maximum)  
0.08 to 0.15
%    
0.25
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
500
MPa  (minimum)  
700 to 850
MPa    
18
% strain  (minimum)  
53
 (minimum)  
 
Other Information
Links