Chemical Composition
0.32 to 0.4
%    
97.8 to 98.7
%    (estimate)
0.7 to 1.1
%    
0.06
%  (maximum)  
0.15 to 0.25
%    
0.15 to 0.35
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Not Applicable
420
MPa    
620 to 770
MPa    
13
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®