Chemical Composition
0.3 to 0.4
%    
0.7 to 1.1
%    
0.3
%  (maximum)  
93.3 to 95.3
%    (estimate)
0.5 to 0.8
%    
0.25 to 0.4
%    
2.75 to 3.25
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.17 to 0.37
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
590
MPa  (minimum)  
755
MPa  (minimum)  
12
% strain  (minimum)  
 
Other Information