Chemical Composition
0.0008 to 0.005
%    
0.27 to 0.33
%    
0.4
%  (maximum)  
97.4 to 98.6
%    (estimate)
1.15 to 1.45
%    
0.025
%  (maximum)  
0.035
%  (maximum)  
0.4
%  (maximum)  
1) Cast analysis.
2) The steel shall be supplied in the killed condition.
3) In the case of grades with specified hardenability requirements, except for P and S, insignificant deviations from the limits for cast analysis are permissible; these deviations shall, however, not exceed in the case of C ±0.01 %, and in all other cases, the values according to ISO 683-1 – Table 4.
4) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulphide morphology) or Pb additions may be available on request. In the first case, the upper limit for the Mn content may be increased by 0.15 %.
5) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
DimensionsYield Strength (MPa)Ultimate Tensile Strength (MPa)Elongation (% strain)
Diameter or thickness, ≤ 16 or ≤ 8 mm respectively≥ 800950 to 1150≥ 13
Diameter or thickness, > 16 to ≤ 40 or > 8 to ≤ 20 mm respectively≥ 650800 to 950≥ 13

650
MPa  (minimum)  
800 to 950
MPa    
13
% strain  (minimum)  
Quenched and tempered (+QT)
Mechanical properties for ruling sections with a diameter > 16 mm to ≤ 40 mm, or for flat products with a thickness > 8 mm to ≤ 20 mm.
 