Chemical Composition
0.2 to 0.3
%    
1.5 to 1.8
%    
0.3
%  (maximum)  
94.5 to 96.7
%    (estimate)
0.3 to 0.6
%    
0.9 to 1.2
%    
0.4
%  (maximum)  
0.03
%  (maximum)  
0.025
%  (maximum)  
0.2 to 0.5
%    
0.2 to 0.3
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
420
MPa  (minimum)  
630
MPa  (minimum)  
16
% strain  (minimum)  
 
Other Information