Chemical Composition
0.0025
%  (minimum)  
0.13
%  (maximum)  
99.3 to 100
%    (estimate)
0.45
%  (maximum)  
0.05
%  (maximum)  
0.05
%  (maximum)  
0.05
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information
Links



No warranty is given for the accuracy of these data