Chemical Composition
0.08
%  (maximum)  
18 to 20
%    
66.9 to 74
%    (estimate)
2
%  (maximum)  
8 to 11
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
310
MPa    
60
% strain    
135
   
 
Other Information
Annealed: 80,000 TS; 45,000 YS; 60 El; 135 HB; Cold drawn: 180,000 TS; 150,000 YS; 10 El; 330 HB; For chemical plant equipment, welded structures; Type 304; stainless, austenitic.
KRUPP V2AS
 