Chemical Composition
0.08
%  (maximum)  
16 to 18
%    
62.2 to 71
%    (estimate)
2
%  (maximum)  
2 to 3
%    
11 to 14
%    
0.75
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
246
MPa    
42
% strain    
 
Other Information
At 70 F: 82,500 TS; 42,300 YS; 55 El; 72 RA; 200 HB; At 1200 F: 53,750 TS; 35,750 YS; 42 El; 55 RA. For heat exchangers, steam piping, high temperature applications; corrosion resistant, austenitic.
CROLOY 16-13-3
 



No warranty is given for the accuracy of these data