Chemical Composition
0.22
%  (maximum)  
0.55
%  (maximum)  
0.35
%  (maximum)  
 
Mechanical Properties
421
MPa    
22
% strain    
149
   
 
Other Information
Cold drawn: 78,000 TS; 68,000 YS; 20 El; 55 RA; 159 HB; Annealed: 73,000 TS; 61,000 YS; 22 El; 58 RA; 149 HB; For gears, bolts, crankshafts, fan blades; water hardened.