Chemical Composition
0.06
%  (maximum)  
18 to 20
%    
69.7 to 73.9
%    (estimate)
0.12 to 0.22
%    
8 to 10
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 