Chemical Composition
0.15
%  (maximum)  
12 to 14
%    
85.3 to 87.9
%    (estimate)
0.6
%  (maximum)  
0.07
%  (minimum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
276
MPa    
30
% strain    
155
   
 
Other Information
Annealed: 75,000 TS; 40,000 YS; 30 El; 60 RA; 155 HB; Heat treated: 200,000 TS; 150,000 YS; 12 El; 40 RA; 415 HB; For screw machine products, valve trim, pump shafts; Type 416, stainless, hardenable.