Chemical Composition
0.25
%    
25
%    
74.8
%    (estimate)
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
345
MPa    
15
% strain    
187
   
 
Other Information
Water quench: 95,000 TS; 50,000 YS; 15 El; 20 RA; 187 HB; For protection tubes, conveyor chains, furnace parts, bolts, nuts, racks; corrosion and heat resistant to S-atmosphere.
BETHADUR NO. 486
 