Chemical Composition
0.15
%  (maximum)  
4 to 6
%    
92.1 to 95.3
%    (estimate)
0.3 to 0.6
%    
0.45 to 0.65
%    
0.5
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
207
MPa    
30 to 100
% strain    
 
Other Information
Annealed: 60,000 TS min; 30,000 YS min; 30 El min; 85 HRB max. Normalized: 160,000 TS; 120,000 YS; 16 El; 34 HRC; Good corrosion resistance, creep strength. Oxidation resistant to 1200 F in air.
B&W CROLOY 5 (T/P 5)
 