Chemical Composition
0.15
%  (maximum)  
2.65 to 3.35
%    
94.3 to 96.3
%    (estimate)
0.3 to 0.6
%    
0.8 to 1.06
%    
0.5
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
207
MPa    
30 to 100
% strain    
 
Other Information
Annealed: 60,000 TS min; 30,000 YS min; 30 El min; 85 HRB max. Better creep properties and corrosion and oxidation resistance than CROLOY 2. Oxidation resistant to 1175 F in air.
B&W CROLOY 3M (T/P 21)
 