Chemical Composition
0.04
%    
11.5
%    
84.1
%    (estimate)
4
%    
0.4
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
731
MPa    
12
% strain    
 
Other Information
Strip Annealed: 123,000 TS; 106,000 YS; 12 El; 28 HRC; At 600 F: 97,700 TS; 89,800 YS; 5 El. For jet engine, missile and space components. Maraging steel, good fracture toughness. Corrosion resistant. Good fabricability.
ALMAR 363
 