Chemical Composition
0.08
%  (maximum)  
13 to 15
%    
82.8 to 87
%    (estimate)
1
%  (maximum)  
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®