Chemical Composition
0.15
%  (maximum)  
8 to 10
%    
87.1 to 90.6
%    (estimate)
0.3 to 0.6
%    
0.9 to 1.1
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
0.25 to 1
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 