Chemical Composition
0.85 to 0.95
%    
17 to 19
%    
0.3
%  (maximum)  
76 to 81.2
%    (estimate)
1
%  (maximum)  
0.9 to 1.3
%    
0.3
%  (maximum)  
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
0.07 to 0.12
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 