Chemical Composition
0.2
%  (maximum)  
23 to 30
%    
67.8 to 77
%    (estimate)
1.5
%  (maximum)  
0.5
%  (maximum)  
0.10-0.25 N2
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
276
MPa    
18 to 100
% strain    
 
Other Information
Annealed: 70,000 TS min; 40,000 YS min; 18 El min; 95 HRB max. Good resistance to oxidation at 1500-2100 F, and resists attack by slag flue dust.