Chemical Composition
0.08 to 0.15
%    
2 to 2.5
%    
95 to 96.5
%    (estimate)
0.4 to 0.7
%    
0.9 to 1.2
%    
0.15 to 0.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 