Chemical Composition
0.22
%  (maximum)  
1.25
%  (maximum)  
0.02
%  (minimum)  
 
Mechanical Properties
310
MPa  (minimum)  
448
MPa  (minimum)  
 
Other Information
V-45 Plate: 65,000 min TS; 45,000 min YS. V-50 Plate: 70,000 min TS; 50,000 min YS. V-55 Plate: 70,000 min TS; 55,000 min YS. V-60 Plate: 75,000 min TS; 60,000 min YS. V-65 Plate: 80,000 min TS; 65,000 min YS.
AW V-STEEL
 



No warranty is given for the accuracy of these data