Chemical Composition
0.17
%  (maximum)  
99.1 to 99.7
%    (estimate)
0.35
%    
0.35
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
379
MPa    
25
% strain    
143
   
 
Other Information
Annealed: 70,000 TS; 55,000 YS; 25 El; 60 RA; 143 HB; Cold drawn: 72,000 TS; 60,000 YS; 22 El; 58 RA; 146 HB; For screws, bolts, gears, shafts, nails, bushings; case hardened.
HUCKINGER KI
 



No warranty is given for the accuracy of these data